Zhongyao Chemical ZHONGYAOTECH
Fire Retardant Materials
Premium Solution

Fire Retardant MaterialsSolutions

Non-Halogen Flame Retardancy Solutions

UL94 V-0 Rating
Achieves highest fla...
Ultra-Low Smoke Density
Smoke density <100, ...
Zero Toxic Release
No halogens or antim...
Scroll to Explore
Industry Overview

Tailored Solutions
for Fire Retardant Materials Industry

As a next-generation halogen-free flame retardant, Mg(OH)₂ decomposes at 340-490°C releasing 31% by weight water vapor, absorbing 1450 J/g heat while forming an MgO protective layer. Compared to traditional halogen/antimony flame retardants, Mg(OH)₂ is non-toxic and non-corrosive, reducing smoke density by 70-80%, fully complying with EU RoHS and REACH regulations. At 55-65% loading in polyolefins, EVA, and unsaturated polyester, it achieves UL94 V-0 rating, meeting stringent fire safety requirements in construction, transportation, and electronics.

01

UL94 V-0 Rating

Achieves highest flame retardancy rating at 55-65% loading

02

Ultra-Low Smoke Density

Smoke density <100, 70-80% reduction vs halogenated FR

03

Zero Toxic Release

No halogens or antimony, compliant with EU regulations

04

Cost-Effective

Abundant raw materials, 30-40% lower cost than brominated FR

Application Scenarios

Real-World Applications

From lab to production line, our solutions have been validated in leading global enterprises

Flame Retardant PE/EVA
01

Flame Retardant PE/EVA

In wire/cable jackets and building pipes, modified Mg(OH)₂ achieves balance between flame retardancy and mechanical properties.

Technical Points

60-65 wt% loading achieves UL94 V-0 (1.6mm thickness)
Impact strength retention >70% (surface modified)
Melt flow index MFI >0.5 g/10min (ensures extrudability)
Limiting oxygen index LOI increased to 28-32%
Modified Mg(OH)2 for Flame Retardant PEModified Mg(OH)2 for LSZH Cables
Intumescent Coatings
02

Intumescent Coatings

In steel structure fire-resistant coatings, Mg(OH)₂ synergizes with APP/MEL systems, providing 2-hour fire resistance.

Technical Points

Expansion ratio 20-30x original thickness
Steel temperature <550°C (120 min flame exposure)
Char layer thermal conductivity <0.1 W/m·K
10-year outdoor weatherability (gloss retention >80%)
Mg(OH)2 for Fire Retardant CoatingsMagnesium Hydroxide
FR Building Materials
03

FR Building Materials

Adding Mg(OH)₂ to decorative panels, insulation materials, and flooring achieves B1-A2 grade fire performance.

Technical Points

Fire rating: GB 8624 B1 / EN 13501 B-s1,d0
Smoke production rate <50% (vs non-FR materials)
Combustion heat value reduced 35-45%
Free of asbestos, halogens and other harmful substances
Magnesium HydroxideModified Mg(OH)2 for Flame Retardant PE
Transportation Interiors
04

Transportation Interiors

High-speed rail, subway, aircraft interiors must meet stringent EN 45545-2 HL2/HL3 standards, Mg(OH)₂ is the preferred choice.

Technical Points

Flame spread ≤1.5m (vertical burn test)
Smoke density Ds <300 (4 minutes)
Toxicity index CITG <0.9
Compliant with EN 45545-2, FAR 25.853 standards
Modified Mg(OH)2 for LSZH CablesModified Mg(OH)2 for Flame Retardant PE

Performance Comparison of Different Flame Retardant Systems

PerformanceMg(OH)₂Al(OH)₃Brominated FRPhosphorus FR
Flame RetardancyUL94 V-0UL94 V-0UL94 V-0UL94 V-1
Loading (wt%)55-6560-7010-2015-25
Smoke Density<100100-150>400150-200
ToxicityNoneNoneHigh (HBr/HCl)Medium (POx)
Decomposition Temp (°C)340-490220-240200-350250-350
Mechanical ImpactMediumLargeSmallMedium
Regulatory ComplianceRoHS/REACHRoHS/REACHRestrictedPartially Restricted

Case Studies

High-Speed Rail Manufacturer: Interior Panel EN 45545-2 Certification

Challenge

PP/PE based interior panels needed EN 45545-2 HL2 rating, original halogenated FR solution was banned.

Solution

Adopted 'Modified Mg(OH)₂ 60% + red phosphorus synergist 5%' halogen-free formula.

Results

  • Flame spread: 1.2m (requirement ≤1.5m)
  • Smoke density Ds: 280 (requirement <300)
  • Toxicity CITG: 0.75 (requirement <0.9)
  • Impact strength retention 65%, meeting installation requirements

Construction Company: External Wall Insulation Material B1 Certification

Challenge

EPS insulation boards needed upgrade from B2 (flammable) to B1 (flame-retardant), traditional HBCD flame retardant was banned.

Solution

Switched to 'Mg(OH)₂ 25% + expandable graphite 10%' composite system.

Results

  • Fire rating upgraded from B2 to B1 (GB 8624)
  • Oxygen index increased from 18% to 28%
  • Thermal conductivity only increased 5% (0.038→0.040 W/m·K)
  • Passed 48-hour boiling water adhesion test

FAQs

Why does Mg(OH)₂ require a high 50-60% loading?
Mg(OH)₂ works through a physical flame retardant mechanism - endothermic decomposition plus water vapor release to suppress flames. Achieving UL94 V-0 requires forming a continuous protective layer, which demands high loading. By comparison, chemical flame retardants (e.g., brominated) work by free-radical capture and are effective at 10-20%.
Will high loading make the material brittle?
Untreated Mg(OH)₂ does reduce impact strength by 40-50%. However, after surface treatment with silane, titanate, or stearic acid, interfacial compatibility with the polymer is greatly improved, and impact strength retention can reach over 70%, meeting most application requirements.
How do I choose between Mg(OH)₂ and Al(OH)₃?
Al(OH)₃ decomposes at 220°C, suitable for low-processing-temperature PVC (160-180°C); Mg(OH)₂ decomposes at 340°C, suitable for PE/PP (180-220°C). Mg(OH)₂ also has higher endothermic heat (1450 J/g vs 1300 J/g), giving better flame retardancy.
How can I improve the flame retardancy efficiency of Mg(OH)₂?
Use synergists: ① red phosphorus 5-8% (gas-phase FR); ② expandable graphite 10-15% (char formation and insulation); ③ zinc borate 3-5% (promotes char formation). With synergists, loading can drop to 45-50% while maintaining V-0.

Industry Trends & Future

1

Global Halogen Ban Accelerating

EU RoHS and REACH strictly restrict halogenated flame retardants. Construction, electronics, automotive industries are shifting to halogen-free solutions like Mg(OH)₂.

2

Nano-Mg(OH)₂ Breaks Loading Bottleneck

Nano-grade Mg(OH)₂ with D50<100nm achieves V-0 at 40-50% loading, maintaining >80% mechanical properties.

3

Composite FR Systems Becoming Mainstream

Mg(OH)₂ + intumescent FR (IFR) + nano-clay ternary synergy achieves integrated flame retardancy, smoke suppression, and low toxicity.

Technical Resources

Ready to Start
Your Project?

Xingtai Zhongyao's technical team has extensive industry experience and can provide professional formula suggestions and technical support based on your specific application needs.

10+
Years Experience
500+
Partner Companies
50+
Export Countries