Zhongyao Chemical ZHONGYAOTECH
Cable Manufacturing
Premium Solution

Cable ManufacturingSolutions

LSZH & Fire-Safe Cable Solutions

Ultra-Low Smoke Density
Smoke density index ...
Zero Halogen Release
Halogen acid release...
High Flame Retardancy
UL94 V-0, LOI value ...
Scroll to Explore
Industry Overview

Tailored Solutions
for Cable Manufacturing Industry

In the cable industry, magnesium hydroxide has become the mainstream choice as an eco-friendly flame retardant. It decomposes at 340-490°C releasing 31% water vapor, absorbing 1450 J/g heat while forming an MgO protective layer that effectively inhibits flame spread. Compared to traditional halogenated flame retardants, Mg(OH)₂ offers zero toxicity and low smoke, meeting stringent life safety requirements for subways, tunnels, and data centers.

01

Ultra-Low Smoke Density

Smoke density index <50, meeting IEC 61034 standard

02

Zero Halogen Release

Halogen acid release <0.5%, complying with IEC 60754-1

03

High Flame Retardancy

UL94 V-0, LOI value increased to 32-35%

04

Excellent Electrical Performance

Volume resistivity >10¹⁴ Ω·cm, voltage resistance >20 kV/mm

Application Scenarios

Real-World Applications

From lab to production line, our solutions have been validated in leading global enterprises

LSZH Power Cables
01

LSZH Power Cables

LSZH cables for subways, tunnels, and high-rise buildings requiring non-toxic smoke and no corrosive gases during fires.

Technical Points

Mg(OH)₂ loading: 60-70 wt% (EVA/EMA matrix)
Smoke density: transmittance >60% (IEC 61034-2)
Oxygen index (LOI): 32-35%
Bending radius: ≤4× cable diameter (maintaining flexibility)
Modified Mg(OH)2 for LSZH CablesMg(OH)2 for PVC Cables
Photovoltaic Cables
02

Photovoltaic Cables

Outdoor 25-year lifespan requiring UV resistance, anti-PID, and flame retardancy.

Technical Points

Ultra-low iron (<10 ppm) prevents EVA yellowing
Nano-scale (D50 <200 nm) maintains transmittance >90%
Hydrophobic treatment, water absorption <0.1%, blocks Na⁺ migration
TÜV 2 PfG 1169/08.2007 certified
Mg(OH)2 for EVA Photovoltaic FilmsModified Mg(OH)2 for LSZH Cables
Railway Cables
03

Railway Cables

Compliant with EN 45545-2 (EU railway fire standard) HL2/HL3 levels with extremely stringent requirements.

Technical Points

Flame spread: ≤1.5 m (single vertical burn test)
Smoke rate: <150 m²/s (cone calorimeter)
Toxicity index (CITG): <0.9
Formula: Mg(OH)₂ 65% + ATH 10% + synergist
Modified Mg(OH)2 for LSZH CablesMgO for Rubber Sheathed Cables
Marine Cables
04

Marine Cables

High salt spray, high humidity, and fire resistance in marine environments requiring special formula design.

Technical Points

Salt spray: 1000h without insulation degradation (IEC 60068-2-11)
Seawater immersion: >30 days maintaining electrical performance
Flame retardancy: IEC 60332-3C bundled burning passed
Low-temp flexibility: -40°C bending without cracking
MgO for Rubber Sheathed CablesModified Mg(OH)2 for LSZH Cables
Recommended Products

Professional Product Series

Mg

Modified Mg(OH)2 for LSZH Cables

Cable Industry

LSZH-certified Mg(OH)₂ (D50 1.2μm, soluble Na <0.01%) delivering smoke density <50, halogen acid <0.5%, and 72h water treeing resistance at 12 kV.

Why Recommended

D50 1.2μm ultrafine, soluble Na <0.01%, developed specifically for LSZH formulations

View Details
Mg

Mg(OH)2 for EVA Photovoltaic Films

Solar Energy

PV-grade Mg(OH)₂ (Fe <10 ppm, D50 nano-scale) maintaining >90% light transmittance, anti-PID performance, and 25-year UV stability in EVA encapsulants.

Why Recommended

PV-grade purity, Fe <10 ppm, 25-year UV resistance without yellowing, excellent anti-PID

View Details
Mg

MgO for Rubber Sheathed Cables

Cable Industry

Cable-grade MgO delivering 20+ kV/mm dielectric strength, UV aging resistance (5000h no cracking), and processing safety for mining/marine rubber cables.

Why Recommended

Dielectric strength 20+ kV/mm, 60-80 m²/g activity, for mining rubber-sheathed cables

View Details
Mg

Mg(OH)2 for PVC Cables

Cable Industry

PVC-compatible Mg(OH)₂ neutralizing 90%+ HCl during combustion, extending heat stability time by 50%, and reducing smoke density 30-40% vs PVC alone.

Why Recommended

Synergistic PVC heat stabilizer, neutralizes 90%+ HCl, reduces smoke density 30-40%

View Details
Mg

Modified Mg(OH)2 for Flame Retardant PE

Flame Retardants

Silane/stearate-modified Mg(OH)₂ achieving 60 wt% loading in PE with <30% impact loss, MFI >0.5 g/10min, and UL94 V-0 at 1.6mm thickness.

Why Recommended

Silane/stearic acid surface treatment, impact strength retention >70% at 60% loading

View Details

Performance Comparison of Flame Retardants in Cables

PropertyMg(OH)₂Al(OH)₃Halogen FRRed Phosphorus
Decomposition Temp (°C)340-490220-240200-300260
Smoke Density Index<5060-80>400100-150
Halogen Acid ReleaseZeroZeroHigh (HCl/HBr)Zero
Loading (wt%)60-6560-6515-2510-15
Impact Strength EffectMediumHighLowLow
Eco-friendlinessExcellentGoodPoor (Toxic)Medium (Moisture Decomp.)
Cost Index1.00.80.61.5

Case Studies

Metro Company: Full-line LSZH Cable Retrofit

Challenge

Original PVC cables did not meet new GB/T 19666 standard, requiring full replacement with LSZH cables.

Solution

Adopted Xingtai Zhongyao 'Modified Mg(OH)₂ LSZH Compound' with EVA matrix formulation.

Results

  • Smoke density reduced from PVC's 350 to 45 (68% transmittance)
  • Halogen acid release from 2.3% to 0.03% (IEC 60754-1)
  • Flame retardancy achieved B1 rating (GB 8624)
  • Installation time reduced 20% (flexible material, easy laying)

PV Manufacturer: EVA Film PID Problem Solution

Challenge

Modules showed 15-20% power degradation after 2 years (PID phenomenon), sodium ion migration detected.

Solution

Added 'PV-grade Mg(OH)₂' (Fe <10 ppm, hydrophobic treatment) to EVA formulation.

Results

  • Water absorption reduced from 0.8% to 0.05%
  • PID test (-1000V, 85°C, 96h) power degradation <2%
  • Transmittance maintained at 91.5% (vs 91.2% before)
  • Zero PID complaints within 25-year warranty

FAQs

Why do LSZH cables require 60-70% high loading?
Mg(OH)₂ uses physical flame retardancy (heat absorption + water release), unlike halogen FR's chemical radical trapping. UL94 V-0 requires sufficient loading to form continuous protective layer. Below 55% fails vertical burn test.
Will high loading make cables too rigid and prone to breaking?
Unmodified Mg(OH)₂ does make materials brittle. But after silane/stearic acid surface treatment, interface bonding with EVA/EMA improves 3-5×, impact strength retention reaches 70%, meeting cable bending requirements.
Why do PV cables emphasize iron content <10 ppm?
Iron ions catalyze EVA degradation and yellowing under UV radiation, reducing transmittance. During 25-year service life, each 1% transmittance drop causes ~0.5% module power loss. Ultra-low iron is key to long-term performance.
How to choose between Mg(OH)₂ and Al(OH)₃?
Al(OH)₃ decomposes at 220°C, unsuitable for PE/PP (processing temp 180-200°C); Mg(OH)₂ decomposes at 340°C, wider processing window. But Mg(OH)₂ has slightly higher moisture absorption, requiring better packaging and storage. Costs are similar.

Industry Trends & Future

1

Ultra-Low Smoke Requirements for Data Center Cables

Next-gen data centers require smoke density <30 (vs traditional <50), driving development of nano-scale Mg(OH)₂ and synergists.

2

Fast-Charging Adaptability for EV Charging Cables

350 kW ultra-fast chargers reach 500A current, cable temp up to 90°C. Requires Mg(OH)₂ + inorganic filler compounding for both flame retardancy and thermal conductivity.

3

Long-Lifespan Requirements for Submarine Cables

30-year maintenance-free design requires Mg(OH)₂ surface encapsulation technology to completely block moisture ingress and prevent long-term hydrolysis.

Technical Resources

Ready to Start
Your Project?

Xingtai Zhongyao's technical team has extensive industry experience and can provide professional formula suggestions and technical support based on your specific application needs.

10+
Years Experience
500+
Partner Companies
50+
Export Countries